Nghiên cứu khả năng hòa tách quặng uran bằng phương pháp cacbonat
Abstract
Two techniques are used for leaching uranium ores - acid leaching using mainly sulfuric acid and alkaline (using a mixture of sodium carbonate and bicarbonate). Alkaline leaching is particulary advantageous in the treatment of the ores with high content of carbonate minerals, since these minerals are not attacked by carbonate solutions. The effect of oxidants, grind size, carbonate concentration and leaching time on the efficiency of uranium recovery from the ores containing 3.5% of carbonate was investigated. Journal of Chemistry, T. 42 (1), Tr. 43 - 46, 2004 Full text of article is in Vietnamese.Downloads
Download data is not yet available.
Published
2007-07-29
Issue
Section
Articles1